Semi-Metal Gasket

SPIRAL WOUND GASKET - STANDARD

- No rings and consists only of Hoop and Filler (Filler Material : Graphite, Teflon..)

- Grafoil Tape No Oxidation range -200~800℃

- Oxidation range-200 ~ 400 ℃

- Applicable Standard: KS B 1518, JIS F 7102 450 SU, JIS F 7102 520 SU, JPI 7S-41-85, API 601-82

SPIRAL WOUND GASKET - OUTER RING

- Spiral wound Gasket with beaded metal strip with outer ring. Soft filler (Graphite strip or PTFE strip) filled between metal strips jutting out on both sides.

- Grafoil Tape No Oxidation -200~800℃

- Oxidation -200 ~ 400 ℃

- Teflon Tape 260℃

- Applicable Standard: KS B 1518, JIS F 7102 450 SU, JIS F 7102 520 SU, JPI 7S-41-85, API 601-82

SPIRAL WOUND GASKET - INNER RING

- Spiral wound Gasket with beaded metal strip, with inner ring Soft filler (Graphite strip or PTFE strip) filled between metal strips jutting out on both sides.

- The Gasket can be used on Male & Female flange

- Grafoil Tape No Oxidation -200~800℃

- Oxidation -200 ~ 400 ℃

- Teflon Tape 260℃

- Applicable Standard: KS B 1518, JIS F 7102 450 SU, JIS F 7102 520 SU, JPI 7S-41-85, API 601-82

DOUBLE JACKETED GASKET

- Double Jacketed Gaskets consist of a metal jacket formed around a soft filler material

- Double Jacketed Gaskets are used on boiler and heat exchanger applications when ample bolting is available to correctly seat the gasket.

- They are designed for high pressure and temperature applications up to and inclusive of Class 900.

- Gasket widths as narrow as 8mm (5/16") can be manufactured dependent on diameter. Very large gasket diameters can also be produced

- Soft iron, steel, SS316, SS304, SS321, SS410, brass, copper, monel

- Filler: Graphite,PTFE,Nonasbestos